The invention relates to a cobalt-base superalloy with the following chemical composition (in % by weight): 25-28 W, 3-8 Al, 0.5-6 Ta, 0-3 Mo, 0.01-0.2 C, 0.01-0.1 Hf, 0.001-0.05 B, 0.01-0.1 Si, remainder Co and unavoidable impurities. This superalloy is strengthened by .gamma.' dispersions and further dispersion mechanisms and has not only good oxidation properties but also, inter alia, improved strength values at high temperatures as compared with cobalt-base superalloys known from the prior art.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

High-temperature-resistant cobalt-base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with High-temperature-resistant cobalt-base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High-temperature-resistant cobalt-base superalloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1808160

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.