Process for the production of a high tenacity propylene polymer fiber which comprises: - spinning fiber from a molten propylene polymer composition consisting essentially of an olefin polymer (I) and a high molecular weight propylene polymer (II) having a branching index less than 1 and melt strength from 5 to 40 cN; said propylene polymer (II) being present in a concentration from 0.1 to 10% by weight with respect to the total weight of the composition; and - drawing the solid fiber thus obtained with a draw ratio greater than 4.5 when the spinning step is continuous and greater than 5 when the spinning step is discontinuous.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

High tenacity propylene polymer fiber and process for making it does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with High tenacity propylene polymer fiber and process for making it, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and High tenacity propylene polymer fiber and process for making it will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1600619

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.