C - Chemistry – Metallurgy – 22 – C
Patent
C - Chemistry, Metallurgy
22
C
C22C 19/05 (2006.01)
Patent
CA 2148290
This invention relates to a hot corrosion resistant nickel-based superalloy comprising the following elements in percent by weight: from about 11.5 to about 13.5 percent chromium, from about 5.5 to about 8.5 percent cobalt, from about 0.40 to about 0.55 percent molybdenum, from about 4.5 to about 5.5 percent tungsten, from about 4.5 to about 5.8 percent tantalum, from about 0.05 to about 0.25 percent columbium, from about 3.4 to about 3.8 percent aluminum, from about 4.0 to about 4.4 percent titanium, from about 0.01 to about 0.06 percent hafnium, and the balance nickel plus incidental impurities, the superalloy having a phasial stability number N V3B less than about 2.45. Single crystal articles can be suitably made from the superalloy of this invention. The article can be a component for a gas turbine engine and, more particularly, the component can be a gas turbine blade or gas turbine vane.
Cannon-Muskegon Corporation
Erickson Gary L.
Ogilvy Renault Llp/s.e.n.c.r.l.,s.r.l.
LandOfFree
Hot corrosion resistant single crystal nickel-based superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Hot corrosion resistant single crystal nickel-based superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hot corrosion resistant single crystal nickel-based superalloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1742118