ABSTRACT OF THE DISCLOSURE The softening temperature or heat resistance of a hot melt composition containing an ethylene-vinyl acetate copolymer and/or rubber is improved by blending an oxidized low molecular weight propylene-ethylene copolymer having a molecular weight of 500 - 10,000, an acid value of 1 - 20 and an ethylene content of 1 - 20 weight % with the ethylene-vinyl acetate copolymer and/ or rubber in a weight ratio of 1/100 - 60/10 relative to the weight of ethylene-vinyl acetate copolymer and/or rubber. The ethylene-vinyl acetate copolymer has a vinyl acetate content of 10 - 45 weight percent and a melt index of 1 - 1,000 g/10 min., the rubber having a mooney viscosity at 25-C of 1 - 20. The composition also includes at least one additive selected from the group consisting of a tackifier, wax and asphalt.

245186

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Hot melt composition having improved softening temperature does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Hot melt composition having improved softening temperature, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hot melt composition having improved softening temperature will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-281532

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.