CA 2436475

A pretreatment method for increasing the average pore size of a catalyst support is disclosed which increases the diffusivity and effectiveness factor .eta.. The pretreatment method includes calcining the support in moisturized air at an elevated temperature sufficient to increase the average pore size. In some embodiments, the support may be treated with an acidic/basic solution prior to the calcination step. Alternatively, the calcination step may occur in a gas mixture including water/air/acidic (or basic) gases.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Hydrothermal pretreatment for increasing average pore size... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Hydrothermal pretreatment for increasing average pore size..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Hydrothermal pretreatment for increasing average pore size... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1354204

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.