C22F 1/04 (2006.01) C22C 21/00 (2006.01)
Patent
CA 2157377
Strength and ductility for aluminum-lithium alloy wrought product in the transverse direction is improved by subjecting these types of alloys to improved T8 temper practice. The wrought product, after solution heat treating and quenching is subjected to a multiple step stretching sequence prior to aging, the total percent reduction for the multiple step stretching sequence ranging between 1 and 20 percent reduction. In the multiple step stretching sequence, each of the stretching steps may have the same or different amounts of percent reduction to achieve the desired total percent reduction. An aluminum-lithium alloy wrought product subjected to the improved T8 temper practice has increased tensile yield stress and percent elongation in its transverse direction to facilitate commercial application of the product in high strength applications.
Bereskin & Parr
Mccook Metals Llc
LandOfFree
Improving mechanical properties of aluminum-lithium alloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Improving mechanical properties of aluminum-lithium alloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Improving mechanical properties of aluminum-lithium alloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1415458