CA 1067702
LOW COST METHOD OF FLUIDIZING CUPOLA SLAG (B) ABSTRACT OF THE DISCLOSURE A composition and method is disclosed for fluxing and fluidizing the slag in an acid-operated cupola, the method comprising adding to the charge therein a fluxing material effective to provide, by weight analysis of the slag, 30 to 42% CaO, 41 to 44% SiO2, 7 to 15% Al2O3, 0.5 to 4.0 TiO2, 1.6 to 3.2% MnO, less than 0.05% P2O5 and less than 1% sulfur. A fluxing composition is disclosed which is comprised by weight percentage of the metal charge comprising, when used with a limestone or a dolomitic limestone charge:. 1.5 to 3.5% limestone or dolomitic limestone and 0.5 to 1.5% FeO Fe2O3 Tio2.
236600
LandOfFree
Low cost method of fluidizing cupola slag (b) does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low cost method of fluidizing cupola slag (b), we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low cost method of fluidizing cupola slag (b) will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-939111