The present invention relates to a low-density nickel-base superalloy comprising the following elements (percent by weight): 7-13% Chromium, 0-16% Cobalt, 2-5% Titanium, 4.5-7% Aluminium, 0-5% Tantalum, 0-2% Hafnium, 0-3% Tungsten, 0-2% Vanadium, 0-5% Molybdenum, 0.06-0.12% Carbon, 0.01-0.03% Boron, 0.005-0.02% Zirconium, nickel and residual impurities, to its use and to the process for obtaining it.
Estolaza Zamora Koldo
Hernandez Aguirre Inigo
Madariaga Rodriguez Inaki
Subinas Rapp Amaia
Industria de Turbo Propulsores S.a.
Sim & Mcburney
LandOfFree
Low-density directionally solidified single-crystal superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low-density directionally solidified single-crystal superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low-density directionally solidified single-crystal superalloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1908010