Abstract of the Disclosure Nickel-iron and nickel-iron-cobalt alloys contain chromium and gamma-prime hardening elements in proportions balanced according to special compositional relationships providing desired thermal expansion, inflection temperature, strength and ductility characteristics, particularly including notch strength needed in machinery and structures subjected in use to varying temperatures and thermal gradients where operating temperatures become elevated above 500°F.
275224
Clatworthy Edward F.
Smith Darrell F. Jr.
Wenschhof Donald E. Jr.
Inco Limited
Smart & Biggar
LandOfFree
Low expansion superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low expansion superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low expansion superalloy will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-860288