Low modulus room temperature vulcanizable silicone elastomer...

C - Chemistry – Metallurgy – 08 – L

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

400/4103, 400/53

C08L 83/08 (2006.01) C08L 83/04 (2006.01) C09K 3/10 (2006.01)

Patent

CA 1055181

Abstract of the Disclosure A one package low modulus room temperature vulcanizable silicone elastomer composition is obtained by mixing 100 parts by weight of a hydroxyl endblocked polydi- methylsiloxane, 0 to 150 parts by weight of a non-acidic, noin-reinforcing filler, 2.5 to 10 parts by weight of Image in which R is methyl or phenyl, 1.5 to 6 parts by weight of an aminoxysilicon compound having 3 to 10 aminoxy groups per molecule, and 1 to 5 parts by weight of N,N-dimethyl- formamide, acetonitrile, or N-n-butylacetamide. The low modulus silicone elastomer is useful in building construction. The composition has improved slump characteristics at low temperatures.

248454

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Low modulus room temperature vulcanizable silicone elastomer... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low modulus room temperature vulcanizable silicone elastomer..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low modulus room temperature vulcanizable silicone elastomer... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-358689

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.