Low-odor, higher molecular weight polyether polyols are produced by purifying the polyether polyols at temperatures of l10 to 150°C and pressures of 10 to 70 hPa with the addition of 5 to 30% by weight of water, wherein the water is passed in finely divided form, with a droplet diameter of about 5 to 100 µ, through the polyether polyols to be purified for a time of metered addition of 1 to 5 hours.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Low-odor, higher molecular weight polyether polyols, a... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Low-odor, higher molecular weight polyether polyols, a..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low-odor, higher molecular weight polyether polyols, a... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1698379

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.