TITLE Low Shrinkage, High Tenacity Poly(.epsilon.-caproamide) Yarn and Process for Making Same ABSTRACT OF THE DISCLOSURE A polyamide yarn is disclosed which is at least about 85% by weight poly(.epsilon.-caproamide) and which has a relative viscosity of greater than 50, a tenacity of at least about 9.3 g/d, a dry heat shrinkage at 160°C of less than about 3 percent, a modulus of at least about 20 g/d, a toughness of at least about 240 g/d?%, a crystal perfection index of greater than about 82, and a long period spacing of greater than about 100 .ANG.. The process for making the yarn includes drawing of a feed yarn while heating to at least about 185°C in at least a final draw stage to a draw tension of at least 4.8 g/d, subsequently decreasing the tension while heating to at least about 185°C to produce a length decrease of between about 13.5 and about 30%, and cooling and packaging the yarn. Doc. J.6
Clark Thomas R. III
Cofer Joseph A. Jr.
Mochel Alan R.
Clark Thomas R. III
Cofer Joseph A. Jr.
E.i. Du Pont de Nemours And Company
Mochel Alan R.
Sim & Mcburney
LandOfFree
Low shrinkage, high tenacity poly(epsilon-caproamide) yarn... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low shrinkage, high tenacity poly(epsilon-caproamide) yarn..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low shrinkage, high tenacity poly(epsilon-caproamide) yarn... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1886682