ABSTRACT LOW THERMAL EXPANSION SUPER ALLOY Disclosed is a nickel-base alloy having a low coefficient of thermal expansion and a high degree of corrosion and oxidation resistance for use without a coating. The high strength alloy is not notch sensitive under impact and has very short term ordering to A2B structure in aging. The alloy nominally contains, in weight percent, 8 chromium, 25 molybdenum, about .003 boron, about 1 iron, about 0.5 manganese, about 0.4 silicon and the balance nickel plus normal impurities.
572026
Rothman Michael F.
Tawancy Hani M.
Haynes International Inc.
Ogilvy Renault Llp/s.e.n.c.r.l.,s.r.l.
LandOfFree
Low thermal expansion superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Low thermal expansion superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Low thermal expansion superalloy will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1283542