A47B 13/08 (2006.01) B32B 17/10 (2006.01)

Patent

CA 2327116

A manufacturing process of a patio tabletop glass with broken protection includes the steps of fully cleaning at least a top surface of a tempered glass layer which has a central hole thereon, drying the cleaned tempered glass layer, heating the entire tempered glass layer to a temperature between 45°C to 65°C; evenly applying a layer of acrylic adhesive on the top surface of the tempered glass layer which temperature is maintained between 45°C to 65°C to form the adhesive layer; attaching the protection layer on the tempered glass layer, cutting excessive edges of the protection layer to a size identical to the tempered glass layer; and forming a center hole on the protection layer, which coaxially aligns with the central hole of the tempered glass layer. Accordingly, even when the patio table top is broken into pieces and particles, the broken glass pieces and particles will not be breaking apart and remain attaching to a protection layer.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Manufacturing process of patio tabletop glass with broken... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Manufacturing process of patio tabletop glass with broken..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Manufacturing process of patio tabletop glass with broken... will most certainly appreciate the feedback.