C - Chemistry – Metallurgy – 22 – C
Patent
C - Chemistry, Metallurgy
22
C
75/14, 53/49
C22C 1/00 (2006.01) C22C 30/04 (2006.01) C22C 33/00 (2006.01)
Patent
CA 1119844
ABSTRACT Lead bismuth and tellurium and/or sulfur are added to steel, to increase the machinability of the steel, in an addition alloy consisting essentially of 5-40 parts lead, 5-40 parts bismuth, up to 6 parts tellurium and up to 25 parts sulfur. The alloy contains at least one of the group tellurium and sulfur, and the alloy has a melting point of at least about 400°C (752°F).
347994
Bhattacharya Debanshu
Holowaty Michael O.
Inland Steel Company
Ridout & Maybee Llp
LandOfFree
Method and alloy for introducing machinability increasing... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method and alloy for introducing machinability increasing..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and alloy for introducing machinability increasing... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-111991