ABSTRACT Method and apparatus for inhibiting stress corrosion cracking adjacent weldments in steel workpieces such as stainless steel pipe through generation of a controllable throughwall temperature differential by exposure of one workpiece surface to externally generated radiant heat while maintaining a flow of coolant fluid past the other surface thereof.
Butler Thomas M.
Sancic David
Butler Thomas M.
Sancic David
Sim & Mcburney
LandOfFree
Method and apparatus for inhibiting stress corrosion cracking does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method and apparatus for inhibiting stress corrosion cracking, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and apparatus for inhibiting stress corrosion cracking will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-2069284