B21B 45/06 (2006.01) B21B 1/26 (2006.01) B21B 45/02 (2006.01) B21B 45/08 (2006.01)

Patent

CA 2255248

A plurality of finishing mills for finish rolling a rolled material are located in a row to configure a finishing mill group. First to third surface coolers for cooling surfaces of the rolled material are located on an entry side of each of first, second and third finishing mills of the finishing mill group, and the amount of cooling water jetted at the rolled material by each surface cooler under a command of a controller is set at 4,000 liters/min~m2, whereby the thickness of scale is restricted to 5 µm or less.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method and system for suppressing surface oxide film during... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method and system for suppressing surface oxide film during..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and system for suppressing surface oxide film during... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1930364

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.