-12- Abstract Method for Applying Aluminide Coatings to Superalloys A powder mixture for applying gas phase aluminide coatings to nickel or cobalt base superalloys is described. A preferred mixture consists essentially of Co2Al5, NH4F.HF, and chromium metal. The mixture is substantially free of aluminum oxide.
550804
Milaniak Michael S.
Okawa Clark T.
Olson Walter E.
Ogilvy Renault Llp/s.e.n.c.r.l.,s.r.l.
United Technologies Corporation
LandOfFree
Method for applying aluminide coatings to superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for applying aluminide coatings to superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for applying aluminide coatings to superalloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1258119