CA 1334914
An improved method of chromizing the surface of a ferritic boiler component. An aqueous coating composition is applied to the surface to be chromized, which includes at least 10% by weight of chromium, at least 12% by weight alumina, a binder of ammonium alginate or methyl cellulose, and a halide activator, and in which the weight ratio of chromium to water is greater than 0.7. Alternative embodi- ments involve the application of a halide activator over the top of a previously applied and dried coating that is lacking said halide activator, as well as to the application of multiple layer single component slurry coatings.
554527
Babcock & Wilcox Company The
Ridout & Maybee Llp
LandOfFree
Method for chromizing of boiler components does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for chromizing of boiler components, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for chromizing of boiler components will most certainly appreciate the feedback.