B - Operations – Transporting – 32 – B
Patent
B - Operations, Transporting
32
B
B32B 17/10 (2006.01) B65D 23/08 (2006.01) C03C 17/00 (2006.01) C03C 17/32 (2006.01) C08J 7/18 (2006.01) C09D 133/10 (2006.01) C09D 143/04 (2006.01)
Patent
CA 2064785
2064785 9119606 PCTABS00008 A method for enhancing the strength of glass containers is presented wherein the containers are preheated to 500 ·C and coated with the strength enhancement coating within six (6) hours after the heat treatment. In one embodiment, a coating station (26) for the strength enhancing coating is located between the exit from a lehr (18) and a cold end spray station (20). In a second embodiment, the strength enhancing coating station (26) is positioned downstream of the cold end station (20).
Crouse Kenneth L.
Cunningham Wells C.
Davis Michael W.
Ellsworth Timothy E.
Hodge Malcolm H.
Advanced Glass Treatment Systems
Swabey Ogilvy Renault
LandOfFree
Method for enhancing the strength of a glass container and... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for enhancing the strength of a glass container and..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for enhancing the strength of a glass container and... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1359591