WGT-6584 IMPROVED METHOD FOR FINISHING FIBERBOARD UTILIZING A FROTHED PRIME COAT Abstract In a method for prime coating fiberboard products the improvement wherein a foaming agent is added to a conventional aqueous latex based prime coating and the coating aerated to give a frothed prime coating having a consistency of 500 to 750 grams per liter, the frothed coating applied to the board product at a rate of 220 to 320 grams per square meter, and heated to collapse the froth and dry the coating.

376846

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for finishing fiberboard utilizing a frothed prime coat does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for finishing fiberboard utilizing a frothed prime coat, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for finishing fiberboard utilizing a frothed prime coat will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1328564

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.