The present invention provides a method for forming thin films, wherein thin films with a uniform thickness can be formed on substrates as objects such as spheroids, even when the films are formed by conventional film-formation methods using an incident particle beam coming from a specific direction (e.g., evaporation and sputtering). In the method, thin films are formed on substrates such as spheroids with an incident particle beam coming from a particle source located in a specific direction by performing a spin motion together with a swing motion. The spin motion is a rotation of the substrate at a constant angular velocity about the spheroidal axis. The swing motion is a rotational oscillation of the same substrate for rotationally oscillating the axis at a constant cycle in one surface, where the center of the rotational oscillation is in the vicinity of the midpoint between two focal points on the axis of the spheroid. As a result, thin films with a uniform thickness in both the peripheral direction of the substrate and in the rotational axis direction of the spin motion can be formed even on substrates including spheroids.
Hashimoto Naotaka
Kitai Takahiro
Omata Yuuji
Suemitsu Toshiyuki
Yokoyama Masahide
Matsushita Electric Industrial Co. Ltd.
Matsushita Electronics Corporation
Panasonic Corporation
Smart & Biggar
LandOfFree
Method for forming thin film, spheroid coated with thin... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for forming thin film, spheroid coated with thin..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for forming thin film, spheroid coated with thin... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1689676