CA 2614229
The invention pertains to a method for improving filament cohesiveness of chopped aramid fiber including the steps of impregnating a film-forming binding agent into the fiber, drying the fiber, optionally applying a finish to the fiber, and chopping the fiber to pieces of 1 to 16 mm length, characterized in that the fiber prior to applying the binding agent is subjected to a twisting process to obtain a fiber having a twisting level of 10 to 150 tpm and that the chopping of the fiber is performed in a rotary chopper.
L'invention concerne un procédé d'amélioration de la cohésion de filaments de fibres aramides hachées, ledit procédé comprenant les étapes suivantes : imprégner un liant filmogène dans la fibre, sécher la fibre, appliquer éventuellement un apprêt plastique à la fibre, et hacher la fibre en des morceaux de longueur comprise entre 1 et 16 mm, caractérisé en ce que, avant l'application du liant, la fibre est soumise à un procédé de torsion de manière à obtenir une fibre ayant un niveau de torsion compris entre 10 et 150 tpm, et en ce que le broyage de la fibre est effectué à l'aide d'un hacheur rotatif.
Olde Hendrik Berend
Willemsen Stephanus
Norton Rose Or S.e.n.c.r.l. S.r.l./llp
Teijin Aramid B.v.
LandOfFree
Method for improving filament cohesiveness of chopped aramid... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for improving filament cohesiveness of chopped aramid..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for improving filament cohesiveness of chopped aramid... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1802408