A method of manufacturing polymeric material having enhanced structural integrity includes heating the material to a temperature between the material's glass transition temperature and the material's melt temperature. Once heated, the material is highly overstretched in a first direction and moderately. overstretched in a second direction. The material is then held in the overstretched condition while it is allowed to cool to. room temperature. Cooling is followed by reheating to a curing temperature. After curing for a predetermined period, the material is again allowed to cool. The completed material has high polymeric orientation in the first direction and moderate polymeric orientation in the second direction. Therefore, the material is characterized by enhanced structural integrity and absence of pinhole defects common to highly oriented polymeric materials.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for manufacturing a high strength angioplasty balloon does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for manufacturing a high strength angioplasty balloon, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for manufacturing a high strength angioplasty balloon will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1868813

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.