C - Chemistry – Metallurgy – 25 – B
Patent
C - Chemistry, Metallurgy
25
B
204/19
C25B 11/04 (2006.01) C25D 3/12 (2006.01)
Patent
CA 1117463
Abstract of the Disclosure Active cathodes for use in electrochemical processes, for example hydrogen production, are prepared by cleaning and etching the cathodes in 10 to 25% nitric acid for 5 to 10 minutes at 35 to 45°C, and thereafter activating the cathode by galvanic coating in a bath containing 50 to 350 g/l of nickel sulphate-hydrate and 10 to 200 g/l of thiourea at a pH of 3 to 6 and a temperature of 30 to 60°C using a cathodic current density of about0.3 to 6 A/dm2. The cathode remains active for a longer period of time and the coating adheres better to the base material.
297597
Andreassen Knut A.
Harang Hdkon
Holte Johan B.
Widding Karl
Fetherstonhaugh & Co.
Norsk Hydro A.s
LandOfFree
Method for preparing active cathodes for electrochemical... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for preparing active cathodes for electrochemical..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preparing active cathodes for electrochemical... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-225609