A method is used to produce a hydrorefining catalyst containing an inorganic oxide carrier and a hydrogenation-active metal in which pores having pore diameters of not more than 50 nm have a pore volume of not less than 0.4 cm3/g, pores having pore diameters of not less than 50 nm have a pore volume of not less than 0.2 cm3/g, and pores having pore diameters of not less than 1000 nm have a pore volume of not more than 0.1 cm3/g. The method comprises the steps of mixing and forming a pseudo-boehmite powder which has a phase transition temperature to .alpha.-alumina of 1220 to 1240 °C; and calcinating the formed pseudo-boehmite under a condition in which the pseudo-boehmite is converted into .gamma.-alumina.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for preparing hydrogenation purification catalyst does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for preparing hydrogenation purification catalyst, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preparing hydrogenation purification catalyst will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1458433

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.