C - Chemistry – Metallurgy – 23 – C
Patent
C - Chemistry, Metallurgy
23
C
C23C 4/10 (2006.01) C23C 4/04 (2006.01) C23C 14/00 (2006.01) C25C 3/08 (2006.01) F27D 1/16 (2006.01) F27D 99/00 (2010.01)
Patent
CA 2285982
The invention relates to a process for producing a coating having a titanium boride content of at least 80% by weight, in which a coating having a thickness of from 0.1 mm to 1 mm, a porosity of not more than 10% by volume and an oxygen content of less than 1% by weight is applied to the surface of a substrate by plasma spraying in an atmosphere which is virtually or completely free of oxygen, with no metallic powder being added to the spraying powder.
L'invention concerne un procédé de réalisation d'un revêtement contenant au moins 80 % en poids de borure de titane, selon lequel on applique un revêtement compris entre 0,1 et 1 mm d'épaisseur dont la porosité maximale est de 10 % en volume et la teneur en oxygène, inférieure à 1 % en poids, sur la surface de l'élément support, par projection plasma dans une atmosphère approximativement voire entièrement exempte d'oxygène, et où la poudre projetée ne comporte pas de poudre métallique.
Hiltmann Frank
Hornung Michael
Kuhn Heinrich
Seitz Katharina
Sussbrich Stephan
Aventis Research & Technologies Gmbh & Co. Kg
Fetherstonhaugh & Co.
Sgl Carbon Ag
LandOfFree
Method for producing a coating containing titanium boride does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing a coating containing titanium boride, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing a coating containing titanium boride will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1779374