A method for producing a component of a titanium-aluminum base alloy comprising hot isostatically pressing the alloy to form a blank, subjecting the blank to a hot forming by a rapid solid-blank deformation, followed by a cooling of the component to form a deformation microstructure with high recrystallization energy potential, thereafter subjecting the component to a heat treatment in the range of the eutectoid temperature (T eu) of the alloy, followed by cooling in air, to form a homogeneous, fine globular microstructure composed of phases GAMMA, BETA0, ALPHA2 and having an ordered atomic structure at room temperature. This abstract is neither intended to define the invention disclosed in this specification nor intended to limit the scope of the invention in any way.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing a component and components of a... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing a component and components of a..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing a component and components of a... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1344073

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.