Method for producing a piece made from a superalloy based on...

C - Chemistry – Metallurgy – 22 – F

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C22F 1/10 (2006.01) C22C 19/03 (2006.01) C22C 19/05 (2006.01)

Patent

CA 2751681

The invention relates to a method for producing a blank for a piece made from a superalloy based on Ni, wherein an alloy is produced and thermal treatments are carried out, characterised in that: said superalloy contains at least 2.5% of the total as Nb and Ta, a thermal treatment is carried out in a number of steps, a first step between 850 and 1,0000C for at least 20 minutes to precipitate the phase d on the grain joints, a second step at a temperature above that of the first step, permitting a partial dissolution of the phase d obtained in the first step, an aging treatment comprising a third step and optionally one or more supplementary steps at a temperature mower than that of the first step and which permit a precipitation of the hardening phases ?' and ?". The invention further relates to a corresponding piece.

Procédé de fabrication d'une ébauche de pièce en superalliage à base de Ni, selon lequel on élabore un alliage, et on réalise des traitements thermiques, caractérisé en ce que : ledit superalliage contient au moins 2,5% au total de Nb et de Ta; on effectue un traitement thermique, comportant une pluralité de paliers : un premier palier entre 850 et 10000C pendant au moins 20 minutes pour précipiter de la phase .delta. aux joints de grains; un deuxième palier à une température supérieure à celle du premier palier et permettant de réaliser une dissolution partielle de la phase .delta. obtenue lors du premier palier; un traitement de vieillissement comportant un troisième palier et éventuellement un ou des paliers supplémentaires, à une température inférieure à celle du premier palier et permettant de faire précipiter les phases durcissantes .gamma.' et .gamma.". Pièce ainsi obtenue.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing a piece made from a superalloy based on... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing a piece made from a superalloy based on..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing a piece made from a superalloy based on... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1671108

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.