A passthrough method is provided in which the surface of an industrial grade, low-grease precursor made of copper, with a defined surface roughness, is patinated. For this purpose the precursor material, connected as the anode, is passed through an electrolysis bath, containing sodium carbonate and/or sodium hydrogencarbonate as well as sodium sulfite and/or sodium disulfite, with a temperature of 30°C to 90°C and a current density of 1 A/dm2 to 20 A/dm2 as bath parameters, for a residence time of 10 seconds to 12 minutes. The precursor material is rinsed and then moved through a fixing bath at a temperature of 35°C to 95°C for a residence time of 10 seconds to 120 seconds, and lastly, after a further rinsing, is dried. The fixing bath contains at least one of the oxidation agents: hydrogen peroxide (H2O2), potassium chlorate (KCIO3), potassium peroxodisulfate (K2S2O8), potassium permanganate (KMnO4), or copper sulfate (CuSo45H2O).
Hoveling Stefan
Luetic Ruzica
Protzer Helmut
Rode Dirk
G. Ronald Bell & Associates
Km Europa Metal Aktiengesellschaft
LandOfFree
Method for producing brochantite patina on copper does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing brochantite patina on copper, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing brochantite patina on copper will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1629129