A process for producing molten pig iron uses direct reduction of iron ore in a pre-reduction stage followed by a final reduction stage. In the pre-reduction stage iron ore is pre-reduced in a melting cyclone by means of a reducing process gas originating from the final reduction stage. A post combustion occurs in the reducing process gas in the melting cyclone so that said iron ore in said melting cyclone is at least partly melted. The partly melted iron ore passes downwardly into a metallurgical vessel situated beneath the cyclone in which the final reduction takes place by supply of coal and oxygen, thereby forming a reducing process gas. A partial post- combustion occurs in the reducing process gas in the metallurgical vessel by means of said oxygen supplied thereto. The post-combustion ratio of the gas on exiting the metallurgical vessel is not more than 0.55. The coal is supplied directly into the slag layer so that said partial post-combustion in said metallurgical vessel is at least partly effected in the slag layer.
Den Hartog Huibert Willem
Meijer Hendrikus Koenraad Albertus
Hoogovens Staal B.v.
Ridout & Maybee Llp
LandOfFree
Method for producing molten pig iron does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing molten pig iron, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing molten pig iron will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1705695