CA 1151846
ABSTRACT OF THE DISCLOSURE A nickel hydroxlde precipitated from nickel-salt solutions acquires, as an active electrode material for alkaline batteries, a highly favourable specific capacity and a reduced tendency to swelling, as a result of a special drying process which is carried out in two stages. In the first stage, using temperatures between 40 and, at the most 80°C, the water content is reduced to a residual humidity of about 10% by weight and then final drying is carried in a second stage at temperatures between 100 and 160°C thereby greatly reduc- ing recrystallization during the first stage and not affecting the capacity of the compound during high temperature drying in the second stage.
358701
Fetherstonhaugh & Co.
Varta Batterie Aktiengesellschaft
LandOfFree
Method for producing nickel hydroxide does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing nickel hydroxide, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing nickel hydroxide will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-522166