C - Chemistry – Metallurgy – 21 – D
Patent
C - Chemistry, Metallurgy
21
D
148/34
C21D 8/00 (2006.01) C21D 8/08 (2006.01) C21D 8/10 (2006.01) C22C 38/04 (2006.01) C22C 38/54 (2006.01)
Patent
CA 1262226
METHOD FOR PRODUCING STEEL BARS HAVING IMPROVED LOW TEMPERATURE TOUGHNESS AND STEEL BARS PRODUCED THEREBY Abstract of the Disclosure A method for producing steel bars is disclosed, which comprises the steps of: heating a steel to a temperature not exceeding 1000°C, the steel consisting essentially of : C: 0.02 - 0.10%, Si: not greater than 0.5%, Mn: 1.10 - 2.50%, Mo: 0.15 - 0.50%, Nb: 0.010 - 0.100%, Al: 0.010 - 0.100%, Cu: 0 - 0.30%, Ni: 0 - 1.20%, Cr: 0 - 1.20%, Ti: 0 - 0.05%, and B: 0 - 0.0030%, with the balance being iron and incidental impurities; hot-rolling the heated steel into a bar under such conditions that the finishing temperature is not higher than 850°C or 850 - 750°C with the total reduction during hot rolling, preferably in the temperature range between 880°C and the finishing temperature, being at least 60%, preferably the hot rolling for the last 2n passes being carried out using oval-, and round-type calibers with an equal reduction in thickness for each of the 2n passes; and cooling the hot-rolled bar to room temperature.
498404
Adachi Takahiko
Fujita Michitaka
Kawamura Eisuke
Kiyokoba Susumu
Nakasato Fukukazu
Adachi Takahiko
Fujita Michitaka
Kawamura Eisuke
Kiyokoba Susumu
Nakasato Fukukazu
LandOfFree
Method for producing steel bars having improved low... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing steel bars having improved low..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing steel bars having improved low... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1209926