ABSTRACT OF THE DISCLOSURE Kaolin clay is dehydrated at a temperature in excess of about 600°C. and below 980°C. and the dehydrated clay is chlorinated in a gas-solid reaction at elevated temperature to remove colored iron impurities as volatile chlorides. The dehydrated clay is then cooled and reacted with an aqueous solution of sodium hydroxide, optionally containing additional sources of alumina and silica, to produce high purity hydrated sodium aluminosilicates such as sodium zeolite A in the form of white crystals useful as ion exchange materials (water softening agents) in detergent compositions.

270501

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing synthetic sodium aluminosilicate... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing synthetic sodium aluminosilicate..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing synthetic sodium aluminosilicate... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-877841

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.