The rate of formation of carbon on the surfaces of thermal cracking tubes and the production of carbon monoxide during thermal cracking of hydrocarbons are inhibited by the use of cracking tubes treated with an antifoulant, including tin compound, silicon compound and sulfur compounds in the presence of a reducing gas such as hydrogen. Additionally, the concentration of carbon monoxide in a pyrolytic cracking process product stream is reduced by the treatment of the thermal cracking tubes of such process with a reducing gas having a concentration of a sulfur compound.
Brown Ronald E.
Greenwood Gil J.
Harper Timothy P.
Reed Larry E.
Scharre Mark D.
Osler Hoskin & Harcourt Llp
Phillips Petroleum Company
LandOfFree
Method for reducing carbon monoxide in the cracking of... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for reducing carbon monoxide in the cracking of..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for reducing carbon monoxide in the cracking of... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1384499