The surface area of carbonaceous powders can be reduced by mixing a small amount of petroleum or coal tar pitch with the carbonaceous powder and pyrolyzing the mixture. The carbonaceous powder becomes coated with decomposition products of the pitch and the coating can have substantially lower surface area than the original carbonaceous powder. Small amounts of pyrolyzed pitch are involved and the bulk properties of the carbonaceous powder remain virtually unaffected. The method is particularly suitable for reducing the surface area of carbonaceous anode powders for use in non-aqueous rechargeable lithium ion batteries and thereby improves the safety of the batteries.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for reducing the surface area of carbonaceous powders does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for reducing the surface area of carbonaceous powders, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for reducing the surface area of carbonaceous powders will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1442502

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.