ABSTRACT OF THE DISCLOSURE A steel stock consisting, in basic composition, of C ?0.12%, 0.5 - 1.0% Mn, 0.10 - 0.25%Si, p ? 0.015%, S? 0.0020%, Nb ? 0.050%, 0.0010 - 0.0060%Ca and the remainder of Fe and negligible traces of impurities is hot rolled, this hot rolling being finished at a temperature above 870°C. The steel is then rapidly cooled on a runout table at an average cooling rate of from 5°C to 30°C per second, and finally, the steel is coiled at a temperature below 570°C. The steel stock has superior resistance to sour gas.
385309
Murayama Hiroshi
Fetherstonhaugh & Co.
Nippon Steel Corporation
LandOfFree
Method for the manufacture of steel suitable for... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for the manufacture of steel suitable for..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the manufacture of steel suitable for... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-254668