Abstract The method disclosed by which to prepare fine hexag- onal ferrites for use in magnetic recording, is one which consists basically in dissolving a) carbonates or other soluble compounds of an aikaline earth metal such as strontium or barium, b) a carbonate or other soluble compound of cobalt, and c) titanium trichlor- ide, all in a solution of ferric citrate and water, whereupon a polycondensation is brought about by ad- dition of ethylene clycol, and heat is applied to eliminate water and organic matter from the compound. Addition of the alkaline earth metal, the cobalt and the titanium is proportioned precisely on the basis of the stoichimetric properties of the end-product, the formula for which is ReO . (6-x)Fe2O3 . xCoO . xTiO2 where x is the extent to which cobalt and titanium atoms replace iron atoms and Re is the alkaline earth metal. Final application of heat produces crystalliz- ation of the superfine hexaferrite particles.

495813

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for the preparation of fine hexagonal ferrite... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for the preparation of fine hexagonal ferrite..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the preparation of fine hexagonal ferrite... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1232355

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.