CA 2075139
ABSTRACT OF THE DISCLOSURE A method of treating coal. The method comprises passing the coal through a retort having a shell temperature of about 500-1000°F and shock heating the coal to a maximum surface temperature of about 500-1000°F without allowing the coal to become exothermic. The coal is prevented from going exothermic by a combination of factors, including the evaporation of moisture from the shock heated coal, the tendency of coal to absorb heat and maintain a temperature of about 390-570°F until the coal undergoes molecular transformation of comp lex hydrocarbons contained in the coal to simpler forms, and the effects of a cooling blanket gas passed through the shock heated coal. The blanket gas preferably comprises an oxygen lean blanket gas stream containing about 2-8% oxygen by volume. The treated coal exhibits extremely low moisture content and increased BTU value and other improved combustion characteristics.
Adams Robert J.
Smart & Biggar
LandOfFree
Method for treating coal does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for treating coal, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for treating coal will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1866728