Method for treating superalloy castings

C - Chemistry – Metallurgy – 21 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148/10

C21D 1/74 (2006.01) B22D 31/00 (2006.01) C22F 1/10 (2006.01)

Patent

CA 1040515

ABSTRACT OF THE DISCLOSURE A method for treating superalloy castings wherein the portions of the castings which solidify directly against the mold walls comprise a substantially continuous skin. In such castings, defects in the form of material voids, including defects present immediately beneath the skin, are eliminated by the application of heat and pressure. The castings are heated to temperatures sufficient to achieve metal movement, and a pressure of at least about 10,000 psi is applied by means of a surrounding gaseous atmosphere. The heat and pressure applica- tion collapses the material in the area of the voids and con- solidates this material to substantially remove the voids and to thereby improve the performance characteristics of the castings.

229755

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for treating superalloy castings does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for treating superalloy castings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for treating superalloy castings will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-588675

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.