CA 1324820
Abstract Laser jet welding of an outer sleeve to an inner fiber ferrule is expedited by, first, machining a thinned region in the outer diameter of the sleeve. After the ferrule has been inserted in the sleeve, the thinned region permits the laser to fuse through the sleeve and melt part of the ferrule, as is required for laser welding of ferrule for the sleeve. The thinned region is preferably made by using a rotary cutter to cut an axially extending slot in the outer sleeve, which permits a succession of laser welds in the axial direction in the slot. In a preferred embodiment, thinned regions are made on opposite sides of the outer sleeve, and laser welding is performed simultaneously on both sides of the sleeve so as to avoid distortions caused by thermal stress asymmetries.
608698
Coyle Richard James Jr.
Mracek Jaroslav
American Telephone And Telegraph Company
Kirby Eades Gale Baker
LandOfFree
Method for welding relatively small parts does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for welding relatively small parts, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for welding relatively small parts will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1203529