Method of arc welding with reverse side cooling for obtaining highly tough large-diameter welded steel pipes Abstract of the Disclosure There is disclosed a novel arc welding method for manufacture of a welded steel pipe wherein the edges of a steel plate bent into a pipe are welded together on one side for forming a pipe and then the seam line of the thus formed pipe is welded by second welding at the side opposite to the side where the first welding was performed. During such second welding, the weld is cooled forcedly from the side where the first welding was performed. Such forced cooling compensates for any physical effects accompanying the welding and imparts elevated toughness to both the weld metal and the heat affected zone.

258605

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of arc welding with reverse side cooling for... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of arc welding with reverse side cooling for..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of arc welding with reverse side cooling for... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-702618

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.