Herein disclosed is a method of coating an automobile body with a chipping-resisting paint, which comprises the steps of: applying and drying that portion of a top-painted automobile body, which is susceptible to the stone chipping, with a chipping-resisting paint containing, as a chief material, 10 to 20 parts of urethane lacquer and, as a solvent, 60 to 75 parts of isopropyl alcohol, 7 to 12 parts of toluene and 7 to 10 parts of ethyl acetate, to have a dry film thickness of at least 30 µ m; stripping the applied and dried coating film of the chipping-resisting paint after lapse of a predetermined period; and applying and drying the stripped portion again with the chipping-resisting paint. These steps are repeated.
Kono Hirofumi
Sato Noboru
Honda Motor Co. Ltd.
Kirby Eades Gale Baker
LandOfFree
Method of coating automobile body with chipping-resisting paint does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of coating automobile body with chipping-resisting paint, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of coating automobile body with chipping-resisting paint will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1357303