Method of concentration of rebellious oxidized copper ores

B - Operations – Transporting – 03 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

361/3

B03D 1/02 (2006.01) B03D 1/002 (2006.01)

Patent

CA 1289274

Abstract A method comprises preparation of a pulp, its sulphidizing and flotation. Sulphidizing of the pulp is carried out with molten sulphur at a temperature of 115-180°C and pressure 1.5-10 atm. in the presence of sodium sulphate or sodium chloride additives.

514188

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of concentration of rebellious oxidized copper ores does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of concentration of rebellious oxidized copper ores, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of concentration of rebellious oxidized copper ores will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1292579

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.