Method of corrosion protection at pipe junctions

F - Mech Eng,Light,Heat,Weapons – 16 – L

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

F16L 58/02 (2006.01) C23F 17/00 (2006.01) F16L 58/18 (2006.01)

Patent

CA 2045685

A method for providing protection against corrosion of a pipe joint (1) formed by the mating of complementary ends (4, 5) of two pipes comprising the steps of: (a) applying controlled heating to a pipe body which is to be joined to an adjacent pipe, (b) applying to the ends (4,5) of each pipe a protective layer or coating of material (2) to the pipe body by a time/temperature func- tion process, (c) allowing the pipe to cool, (d) bevelling the terminations of the protective layer or coating (2), (e) mating comple- mentary ends (4,5) of the pipes together to form a seated and corrosion resistant joint (1).

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of corrosion protection at pipe junctions does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of corrosion protection at pipe junctions, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of corrosion protection at pipe junctions will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2041629

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.