ABSTRACT OF THE DISCLOSURE A method of increasing the yield of oxidized coal or coal from surface or strip mines by about 23-30% by weight where said coal particles are concentrated by froth flotation. The method consists of utilizing as a promoter or frothing aid about 0.03 - 0.09 lbs/ton of said coal of a water- soluble anionic linear addition polymer of a polymerizable monoethylenically unsaturated compound having an average molecular weight of about 100,000 to 1,000,000 or more with a preferred range of 1,000,000 or more. This method is also utilized where oxidized coal is admixed with a major amount of deep coal amounting up to 80 - 95% and greater by weight of the mixture. A preferred promoter or frothing aid for oxidized coal is sodium polyacrylate and the promoter or frothing aid is used in an aqueous solution or dispersion in preferred operable percentiles of .5 - 1.5% by weight of the solution or dispersion.

283873

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of increasing the yield of oxidized coal in flotation... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of increasing the yield of oxidized coal in flotation..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of increasing the yield of oxidized coal in flotation... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-987639

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.