Method of increasing useful life of tool steel cutting tools

C - Chemistry – Metallurgy – 23 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

204/96.05

C23C 14/46 (2006.01) C23C 14/02 (2006.01)

Patent

CA 1330775

12 Abstract of the Disclosure The wear life of a high-speed tool steel cutting bit is increased by (a) cleansing the bit by subjection to an ion beam; (b) while preventing the temperature of the cleansed bit from rising above 350°C, coating the cleansed bit by condensing sputtered atoms of titanium and boron thereonto, the condensation being carried out to provide a coating thickness of 2-6 microns. An argon or krypton beam of ions is accelerated to 1300-1800 volts as a broad-beam ion source to sputter a titanium diboride target arranged as a cathode. The sputtering is carried out for 5-10 minutes while the bit is heated to about 200°C and a soft vacuum of about 4-6 milli-torr is used during the process.

581523

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of increasing useful life of tool steel cutting tools does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of increasing useful life of tool steel cutting tools, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of increasing useful life of tool steel cutting tools will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1216192

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.