Abstract Of The Disclosure Clarified slurry oil feedstock is heated at tempera- tures above 340°C. and preferably between 390°C. and 410°C. for periods exceeding a minimum of about 2 hours, under reflux conditions and in the absence of air, so as to maximize the polymerization of light ends in the formation of petroleum pitch. An increased yield of petroleum pitch is obtained from the clarified slurry oil feedstock. -1-
261917
Haywood Samuel I.
Ingram Henry T.
LandOfFree
Method of increasing yield of petroleum pitch does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of increasing yield of petroleum pitch, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of increasing yield of petroleum pitch will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-71212