Disclosed herein is a method which enables permanent current junction of a tape-type oxide superconducting wire and suppresses reduction of its critical current. An end portion of a tape-type wire (10) to be joined is removed to expose oxide superconductor filaments. Another tape- type wire (10') to be joined with the wire (10) is processed in a similar manner. The tape-type wires (10, 10') are so superposed that the surfaces exposing the filaments face with each other, and the superposed portions are pressed in a direction perpendicular to principal surfaces of the tapes and heat treated at a temperature of 800 to 900°C, to be completely joined with each other.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of joining superconducting wire using oxide... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of joining superconducting wire using oxide..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of joining superconducting wire using oxide... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2082617

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.