ABSTRACT OF THE DISCLOSURE A method of producing the title composites comprises providing graphite on carbon fibres for example in the form of braids or tows and contacting them with molten silicon at temperatures in the range of about 1400 to 1800°C in an inert atmosphere. The silicon carbide is formed in situ in a time generally within the period 1 - 15 minutes.
198361
Laskow William
Morelock Charles R.
LandOfFree
Method of making a silicon carbide filamentary reinforced... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of making a silicon carbide filamentary reinforced..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making a silicon carbide filamentary reinforced... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-808293